[229] A multiplicative plastic hardening model in consideration of strain softening and strain rate: Theoretical derivation and characterization of model parameters with simple tension and creep test
저자
Kim HK, Yoon JW, Chung K, Lee MG*
저널 정보
Int J Mech Sci, 187, 105913
출간연도
2020
링크
Prev
이전
[228] Modeling differential permanent softening under stain-path changes in sheet metals using a modified distortional hardening model
다음
[230] A virtual fields method for identifying anisotropic elastic constants of fiber reinforced composites using a single tension test: theory and validation
Next
목록 보기