[301] Crystal plasticity study of the effect of asymmetric structure of diffusive film cooling hole on heterogeneous creep and fracture behavior of NBSC superalloy

저자

Zhang Z, Park J et al. Lee MG*

저널 정보

Journal of Materials Research and Technology (JMR&T), 27 (Nov), 5041-5058

출간연도

2023